Synthesis of Barium-zinc-titanate Ceramics
(Međunarodni Institut za nauku o sinterovanju, Beograd, 2012)
Mixtures of BaCO3, ZnO and TiO2 powders, with molar ratio of 1:2:4, were mechanically activated for 20, 40 and minutes in a planetary ball mill. The resulting powders were compacted into pellets and isothermally sintered ...
ZnTiO3 Ceramic Nanopowder Microstructure Changes During Compaction
(Međunarodni Institut za nauku o sinterovanju, Beograd, 2013)
ZnTiO3 nanopowder as a constitutive component in compact production was primarily characterised. Scanning electron micrographs of as received powder were recorded. Mercury porosimetry and nitrogen adsorption were also ...
Analysis and Modeling of Sintering of Sr-hexaferrite Produced by PIM Technology
(Međunarodni Institut za nauku o sinterovanju, Beograd, 2011)
The powder injection moulding (PIM) technology is lately becoming more and more significant due to complex design possibilities and good repeatability. This technology requires optimization of all steps starting with ...
History and challenges of barium titanate: Part I
(Međunarodni Institut za nauku o sinterovanju, Beograd, 2008)
Barium titanate is the first ferroelectric ceramics and a good candidate for a variety of applications due to its excellent dielectric, ferroelectric and piezoelectric properties. Barium titanate is a member of a large ...
Intrinsic resistivity of sintered nickel manganite vs. powder activation time and density
(Međunarodni Institut za nauku o sinterovanju, Beograd, 2008)
In this work the DC resistivity of sintered nickel manganite NiMn2O4 (NTC thermistor material) was studied as a function of additional powder activation time in a planetary ball mill (0, 5, 15, 30, 45 and 60 min). The ...
SiC Synthesis Using Natural Mg-Silicates
(Međunarodni Institut za nauku o sinterovanju, Beograd, 2012)
The silicon carbide powders are prepared by carbothermal reduction of domestic mineral resources (white and brown sepiolite), at relatively low temperatures (1200 - 1600 degrees C). Carbothermal reduction process is greatly ...
Effect of Binder Molecular Weight on Morphology of TiO2 Films Prepared by Tape Casting and Their Photovoltaic Performance
(Međunarodni Institut za nauku o sinterovanju, Beograd, 2012)
Titanium(IV) oxide in the form of anatase has proven to be the best choice for photoanodic material in dye-sensitized solar cells (DSCs). The aim of the work was to study the influence of binder molecular weight on the ...
Optical Properties of CuSe Thin Films - Band Gap Determination
(Međunarodni Institut za nauku o sinterovanju, Beograd, 2017)
Copper selenide thin films of three different thicknesses have been prepared by vacuum evaporation method on a glass substrate at room temperature. The optical properties of the films were investigated by UV-VIS-NIR ...
Sol-gel Synthesis of Anatase Nanopowders for Efficient Photocatalytic Degradation of Herbicide Clomazone in Aqueous Media
(Međunarodni Institut za nauku o sinterovanju, Beograd, 2017)
TiO2 nanopowders were produced by sol-gel technique using TiCl4 as a starting material. For the preparation of crystalline anatase with developed surface area, this aqueous solution has been mixed with 0.05 M or 0.07 M ...
Processing and Properties of Ceramic Yttrium Manganite Sintered by Different Methods
(Međunarodni Institut za nauku o sinterovanju, Beograd, 2021)
Intergranular and intragranular cracks that usually form during sintering of yttrium manganite (YMnO3) ceramic samples hinder the densification process of this ceramic and deteriorate its magnetic and ferroelectric properties. ...