Antiferromagnetism and heat capacity of NaCo2-xCuxO4 ceramics
(Elsevier Sci Ltd, Oxford, 2017)
Polycrystalline samples of NaCo2-xCuxO4 (x=0, 0.01, 0.03 and 0.05) were synthesized in two different ways: 1) by a mechanochemically assisted solid-state reaction method (MASSR) and 2) by a citric acid complex method (CAC). ...
Transformation of Cs-exchanged clinoptilolite to CsAlSi5O12 by hot-pressing
(Elsevier Sci Ltd, Oxford, 2017)
Dense CsAlSi5O12 was successfully obtained by hot pressing of Cs-exchanged clinoptilolite at 900 degrees C. Simultaneous application of high temperature and mechanical pressure allowed formation of CsAlSi5O12 at temperature ...
Hydrothermally assisted synthesis of YMnO3
(Elsevier Sci Ltd, Oxford, 2015)
In this work single phase hexagonal YMnO3 powders were prepared starting from Y(CH3COO)(3)center dot xH(2)O, Mn(CH3COO)(2)center dot 4H(2)O, KMnO4 and KOH using methods of conventional (280 degrees C for 6 h) or microwave ...
Dielectric and ferroelectric properties of Ho-doped BiFeO3 nanopowders across the structural phase transition
(Elsevier Sci Ltd, Oxford, 2017)
We have studied Ho-doped BiFeO3 nanopowders (Bi1-xHoxFeO3, x = 0-0.15), prepared via sol-gel method, in order to analyse the effect of substitution-driven structural transition on dielectric and ferroelectric properties ...
Structure and properties of chemically synthesized BiFeO3. Influence of fuel and complexing agent
(Elsevier Sci Ltd, Oxford, 2015)
Perovskite, single multiferroic bismuth ferrite was prepared by two chemical methods: auto-combustion and soft chemical route. Influence of different fuels and complexing agents and thermal treatment on purity of bismuth ...
Synthesis and characterization of tungsten carbide fine powders
(Elsevier Sci Ltd, Oxford, 2015)
Fine tungsten carbide (WC) powder was prepared by solid state reaction between tungsten powder (W) and activated carbon cloth as a new carbon (C) source. The effect of temperature and time of heat treatment as well as the ...
Dielectric and magnetic properties of BaTiO3-NiFe2O4 multiferroic composites
(Elsevier Sci Ltd, Oxford, 2014)
Multiferroic composites with the general formula x BaTiO3-(1-x) NiFe2O4 (x=0.5, 0.7, 0.8) were prepared by mixing chemically obtained nickel ferrite and barium titanate powders. Optimum processing parameters for a reduction ...
Antimony doping effect on barium titanate structure and electrical properties
(Elsevier Sci Ltd, Oxford, 2011)
Nanopowders of pure and antimony doped barium titanate (BaTiO3-BT) were synthesized by polymeric precursors method based on Pechini process. Obtained powders were pressed and sintered at 1300 degrees C for 8 h. XRD analysis ...
Structural and electrical properties of sintered Fe2O3/TiO2 nanopowder mixtures
(Elsevier Sci Ltd, Oxford, 2014)
Starting nanopowders of TiO2 (anatase 99.7%) and alpha-Fe2O3 (hematite) were mixed in the weight ratios 60:40 and 40:60. Green samples were sintered in the temperature range 750-1250 degrees C in air. Structural, morphological ...
Properties of lanthanum doped BaTiO3 produced from nanopowders
(Elsevier Sci Ltd, Oxford, 2010)
Pure and barium titanate (BT) powders doped with different lanthanum concentration were prepared by the polymeric precursor method (Pechini process) which was carried out as a three-stage process from organometallic ...