Effect of La substitution on the structural and electrical properties of BaBi4-xLaxTi4O15
(Elsevier Sci Ltd, Oxford, 2013)
Pure and lanthanum doped barium bismuth titanate BaBi4-xLaxTi4O15 (BBLT, x=0, 0.05, 0.15, 0.30) ceramics were prepared utilizing solid state method. The X-ray diffraction (XRD) data confirmed formation of single-phase ...
Far infrared and micro structural studies of mechanically activated nickel manganite
(Elsevier Sci Ltd, Oxford, 2013)
Nickel manganite powder synthesized by calcination of a stoichiometric mixture of manganese (MnO Aldrich 99.9%) and nickel oxide (NiO Merck, 99.5%) containing 0.5 wt% CoO and Fe2O3, was additionally mechanically activated ...
Visible-light active mesoporous, nanocrystalline N,S-doped and co-doped titania photocatalysts synthesized by non-hydrolytic sol-gel route
(Elsevier Sci Ltd, Oxford, 2016)
Visible-light active mesoporous N,S-doped and co-doped anatase TiO2 powders were synthesized by non-hydrolytic sol-gel route, starting from TiCl4 and Ti((OPr)-Pr-i)(4) dissolved in cyclohexane or dimethyl sulfoxide, later ...
Antimony doping effect on barium titanate structure and electrical properties
(Elsevier Sci Ltd, Oxford, 2011)
Nanopowders of pure and antimony doped barium titanate (BaTiO3-BT) were synthesized by polymeric precursors method based on Pechini process. Obtained powders were pressed and sintered at 1300 degrees C for 8 h. XRD analysis ...
Properties of lanthanum doped BaTiO3 produced from nanopowders
(Elsevier Sci Ltd, Oxford, 2010)
Pure and barium titanate (BT) powders doped with different lanthanum concentration were prepared by the polymeric precursor method (Pechini process) which was carried out as a three-stage process from organometallic ...
Nanoindentation study of nickel manganite ceramics obtained by a complex polymerization method
(Elsevier Sci Ltd, Oxford, 2016)
The chemical synthesis of nickel manganite powder was performed by a complex polymerization method (CPM). The obtained fine nanoscaled powders were uniaxially pressed and sintered at different temperatures: 1000-1200 degrees ...