Far infrared reflectance of sintered Zn2TiO4
(Springer, New York, 2008)
Zinc-titanate ceramics were obtained by initial mechanical activation in a high-energy planetary mill for 15 min followed by sintering at temperatures 900-1100 degrees C for 2 h. Room temperature far infrared reflectivity ...
Structural analysis of Zn2TiO4 doped with mgo
(Springer New York LLC, 2009)
The starting mixtures of ZnO, TiO2, and MgO (0, 1.25, and 2.5 wt.%) powders are mechanically activated in a high-energy planetary mill for 15 min and then sintered between 800 and 1100 degrees C for 2 h. The influence of ...
The influence of mechanical activation on the stoichiometry and defect structure of a sintered ZnO-Cr2O3 system
(Trans Tech Publications Ltd, 2004)
Mixtures of starting ZnO and Cr2O3 powders in equimolar quantities were mechanically activated by grinding using a high energy vibro-mill for 0, 40 and 80 minutes. Qualitative X-ray diffraction analysis made after sintering ...