Microstructural investigation of the PZT films prepared from the suspension of nanocrystalline powders
(Elsevier Sci Ltd, Oxford, 2004)
PZT thin films of composition Pb(Zr0.52Ti0.48)O-3 were prepared by a novel method from the suspension of nanocrystalline PZT powders. The powders were obtained by mechanochemical synthesis. Films were deposited on silicon ...
Tailoring of morphology and orientation of LaNiO3 films from polymeric precursors
(Elsevier Sci Ltd, Oxford, 2007)
The aim of this work was to prepare lanthanum nickel oxide (LaNiO3, LNO) thin films of different morphology and orientation. The precursor solutions were prepared by a chemical method from citric salts of lanthanum and ...
Nonlinear properties and stability of SnO2 varistors prepared by evaporation and decomposition of suspensions
(Elsevier Sci Ltd, Oxford, 2005)
SnO2 varistors doped with CoO, Cr2O3 and Nb2O5 were prepared by evaporation and decomposition of suspensions. The composition of the varistors was optimized to improve electrical properties, such as nonlinearity, leakage ...
Strontium titanate films prepared by spray pyrolysis
(Elsevier Sci Ltd, Oxford, 2004)
Strontium titanate thin films were prepared by spray pyrolysis technique. Deposition parameters, such as solution concentration, time and temperature of deposition, and flow rate of carrier gas were optimized to obtain ...
Structural, ferroelectric and magnetic properties of BiFeO3 synthesized by sonochemically assisted hydrothermal and hydro-evaporation chemical methods
(Elsevier Sci Ltd, Oxford, 2016)
BiFeO3 powders were synthesized by sonochemically assisted hydrothermal and hydro-evaporation methods. The X-ray diffraction confirmed the presence of secondary phases, Bi25FeO39 and Bi2Fe4O9, in as prepared BiFeO3 powders. ...
Far infrared reflection spectroscopy of Zn2SnO4 ceramics obtained by sintering mechanically activated ZnO-SnO2 powder mixtures
(Elsevier Sci Ltd, Oxford, 2007)
A mixture of starting ZnO and SnO2 powders (molar ratio 2: 1) were mechanically activated for 10, 40, 80 and 160 min in a planetary ball mill and then isothermally sintered at 1300 degrees C for 2 h in order to obtain ...
Far infrared properties of sintered NiO
(Elsevier Sci Ltd, Oxford, 2007)
Far infrared reflection spectra of NiO polycrystals sintered at 1100 degrees C for various times (30-240 min) were measured at room temperature using a FTIR Spectrometer-Brucker 113V. The measured spectra depended on the ...
Multiferroic bismuth manganite prepared by mechanochemical synthesis
(Elsevier Sci Ltd, Oxford, 2010)
Multiferroic bismuth manganite (BiMnO3) is known as a material that exhibits both ferromagnetic and ferroelectric properties making it interesting for various technological applications. Unfortunately, preparation of BiMnO3 ...
Preparation of ultrathin PZT films by a chemical solution deposition method from a polymeric citrate precursor
(Elsevier Sci Ltd, Oxford, 2010)
Ultrathin PZT film was prepared using a chemical solution deposition method from polymeric citrate precursors. The PZT solution was spin-coated on an amorphous silica layer formed on a Si(l 0 0) substrate. The films were ...
Ultra-high breakdown field varistors prepared from individually synthesized nanoprecursors
(Elsevier Sci Ltd, Oxford, 2015)
Previously synthesized nanocrystalline ZnO doped with cobalt and manganese, Bi2O3 and Sb2O3 were the precursors for high voltage varistors preparation. Varistor ceramics were sintered at 750 degrees C, 770 degrees C or 900 ...