Pretraživanje
Prikaz rezultata 1-3 od 3
Far infrared reflectance of sintered Zn2TiO4
(Springer, New York, 2008)
Zinc-titanate ceramics were obtained by initial mechanical activation in a high-energy planetary mill for 15 min followed by sintering at temperatures 900-1100 degrees C for 2 h. Room temperature far infrared reflectivity ...
Synthesis of BaTiO3 from a mechanically activated BaCO3-TiO2 system
(Međunarodni Institut za nauku o sinterovanju, Beograd, 2008)
In this article the solid state reaction of BaTiO3 formation from a mechanically activated BaCO3-TiO2 system has been investigated. An equimolar mixture of BaCO3 and TiO2 powders was activated in a planetary ball mill in ...
Intrinsic resistivity of sintered nickel manganite vs. powder activation time and density
(Međunarodni Institut za nauku o sinterovanju, Beograd, 2008)
In this work the DC resistivity of sintered nickel manganite NiMn2O4 (NTC thermistor material) was studied as a function of additional powder activation time in a planetary ball mill (0, 5, 15, 30, 45 and 60 min). The ...