Prikaz osnovnih podataka o dokumentu
Structural, microstructural and electrical properties of Sb-doped BaSnO3 ceramics
dc.creator | Vukašinović, Jelena | |
dc.creator | Počuča-Nešić, Milica | |
dc.creator | Luković Golić, Danijela | |
dc.creator | Ribić, Vesna | |
dc.creator | Branković, Zorica | |
dc.creator | Dapčević, Aleksandra | |
dc.creator | Bernik, Slavko | |
dc.creator | Branković, Goran | |
dc.date.accessioned | 2023-08-11T10:17:38Z | |
dc.date.available | 2023-08-11T10:17:38Z | |
dc.date.issued | 2019 | |
dc.identifier.isbn | 978-86-912959-5-0 | |
dc.identifier.uri | http://rimsi.imsi.bg.ac.rs/handle/123456789/2071 | |
dc.description.abstract | BaSnO3 (BSO) belongs to the perovskite-type oxides with a cubic crystal structure. It exhibits interesting electrical, optical and photocatalytic properties. BSO has a potential application as transparent conductor, gas sensor, photocatalyst or dielectric capacitor. It is an insulating material with wide band gap (Eg = 3.1–3.4 eV), but its electrical properties can be adjusted by doping with aliovalent cations. In this work, we investigated the influence of antimony (Sb3+), as a dopant, on crystal structure, microstructural and electrical properties of BSO ceramics. Stoichiometric mixture of powders BaCO3, SnO2 and Sb2O3 was mechanochemically activated in a planetary ball mill and afterwards calcined at 900 ºC for 4 h. As-prepared powders were sintered by spark plasma sintering technique (1200 ºC for 5 min) in order to produce ceramic samples BaSn1-xSbxO3 (x = 0.00, 0.04, 0.06, 0.08 and 0.10). All samples were characterized using X-ray Diffraction (XRD) analysis, High Resolution Transmission (HRTEM) and Field Emission Electron Microscopy (FESEM). Electrical conductivity of BaSn1-xSbxO3 ceramics was determined by measuring of the current-voltage (I–U) characteristics in different mediums and at different temperatures. XRD analysis confirmed the existence of cubic BSO, as a dominant phase, and tetragonal Ba2SnO4, as a secondary phase. FESEM analysis revealed homogenous microstructure in all samples and noticeable decrease of the grain size in doped samples compared to BSO. HRTEM micrographs of the undoped sample showed less ordered microstructure with amorphous phase in the grain boundary region. Doped samples revealed much higher crystallinity, especially in the grain boundary regions without presence of defects. Low angle grain boundaries (LAGB) are observed (the angle equals 2.08°) on the HRTEM micrographs of BaSn0.92Sb0.08O3. It was observed that all doped samples are n-type semiconductors, having linear I–U characteristics up to 150 °C. Sample BaSn0.92Sb0.08O3 showed the highest conductivity, most likely due to the presence of the LAGB, which allow easier charge carrier transfer between grains and greater carrier mobility [1]. [1] Y. Furushima, A. Nakamura, E. Tochigi, Y. Ikuhara, K. Toyoura, K. Matsunaga, J. Appl. Phys., 120 (2016) 1421071–1421079. | sr |
dc.language.iso | en | sr |
dc.publisher | Serbian Crystallographic Society | sr |
dc.relation | Ministry of Education, Science and Technological Development, Republic of Serbia | sr |
dc.rights | openAccess | sr |
dc.source | 26th Conference of the Serbian Crystallographic Society, June 27-28, 2019, Silver Lake, Serbia | sr |
dc.subject | BaSnO3 | sr |
dc.subject | Spark plasma sintering | sr |
dc.subject | XRD analysis | sr |
dc.subject | HRTEM | sr |
dc.subject | Low angle grain boundaries | sr |
dc.subject | Linear I–U characteristics | sr |
dc.title | Structural, microstructural and electrical properties of Sb-doped BaSnO3 ceramics | sr |
dc.type | conferenceObject | sr |
dc.rights.license | ARR | sr |
dc.citation.epage | 73 | |
dc.citation.spage | 72 | |
dc.identifier.fulltext | http://rimsi.imsi.bg.ac.rs/bitstream/id/5465/bitstream_5465.pdf | |
dc.identifier.rcub | https://hdl.handle.net/21.15107/rcub_rimsi_2071 | |
dc.type.version | publishedVersion | sr |